Electronic Sealant Silicone Rubber

Type: Silicone Ink
Printing Type: Embedment
Ink Drying: Heat Curing
Performance: Viscosity
Component: Liquid Silicone
Application: Electronic Component Seal
Customization:
Gold Member Since 2019

Suppliers with verified business licenses

Manufacturer/Factory

Basic Info.

Model NO.
THR-127
Color
Black /White
Ink Type
Silicone Ink
Certificate
Oeko-Tex100 & SGS
Package
20kg/Barrel
Shelf Life
1 Year Room Temperature Sealed
Transport Package
Sea/Air
Specification
20kg/barrel
Trademark
Tinhui
Origin
Guangdong China
HS Code
3910000000
Production Capacity
100 Ton/Month

Product Description

Overview, this product is a one-component, neutral silicone adhesive, belongs to the dealcohol system, in the role of water vapor in the air curing, curing into a certain toughness, strength of elastic rubber, high and low temperature resistance, it keeps elasticity and stability in-55 ~ 180 °C for a long time, and has excellent aging resistance and weather resistance. Due to the alcohol released during the curing process, it has no corrosion to copper and other materials, and no irritating gas released, it belongs to environmental protection products
Electronic potting silica gel
  THR-1271D THR-1271E THR-1271F THR-1271M THR-1271R
Project   index
Before cuing Appearance Translucent paste Transparent flowing White White paste Red paste
Extruded velocity(g/3s) 10-30 ≥60 ≥10 ≥30 ≥30
Surface dry time(min)(min) 2-10 2-15 2-20 5-15 5-15
 After   curing   time Hardness (Shore A) 14-18 8-15 20-30 25-35 20-30
Tensile stength(MPa) ≥0.6 ≥0.5 ≥1.0 ≥1.5 ≥1.5
elongation(%) ≥300 ≥250 ≥200 ≥400 ≥500
Tear strength(kN/m) ≥3.5 ≥1.5 ≥3.0 ≥8.0 ≥8.0
idensity(g/cm3) 1.05±0.05 1.05±0.05 1.4±0.5 1.35±0.05 1.35±0.05
  Heat conductivity (W/mk) - - 0.45 - -




Properties under the action of Water Vapor in the air, the room temperature curing system of debonding cured into elastic rubber with certain toughness has excellent adhesion to most substrates, application field for various types of electronic components of bonding and sealing, use method 1. Clean the surface: to be glued or coated surface clean, remove rust, dust and oil, etc. . 2. SIZING: extrude the product to the cleaned surface, make it evenly distributed, and fix it by the adhesive surface. 3. Curing: The glued part is exposed to air to cure it. This product is cured from the outside to the inside of the curing process, 24 hours (25 °C, 50% relative humidity) curing depth of 2-4 mm. If the temperature is low, humidity small curing time will be extended.





It can be applied to PC (poly carbon), PP, ABS, PNC and other materials and metal surfaces. It has excellent adhesion performance and fully meets the requirements of European ROHS directive. The electronic potting adhesive is resistant to high and low temperature (- 50c-2500), water, oxygen and weather aging. It can keep its elasticity at low temperature (- 50). It also has the properties of corrosion resistance and quenching, and has strong adhesion; It has a strong fixation effect on Qingguang panel, solar cell and electronic components. It is used as the sealing material of electronic and electrical components. It has the nature of anti shock and weather resistance and is used as the sealing, bonding and coating materials of electronic components. It also has the functions of moisture-proof, insulation, shockproof and natural resistance. Backlight, high voltage module, conversion line HD lamp module power supply, automobile power supply network transformer, communication element, household electricity, solar cell, solar cell transformer and electronic element can be well responded to


Operation method of electronic sealer:


1. Weigh the weight ratio of component A and component B: measure correctly according to the correct mix proportion (weight ratio). If there is a large error in the measurement of mix proportion, the product characteristics will not be displayed well

2. Mix semi-uniform silica gel and curing agent: mix component A and component B semi uniformly. When mixing AB glue, pour the part with less proportion into the part with more proportion for mixing. When mixing the resistance, it should be smooth and not too decisive. Hold for about 3 minutes. Mix the bottom, wall and other parts of the container evenly. If not, the curing will be incomplete. The container must be semi glue

3. Vacuumize and discharge bubbles: move to the vacuum box quickly after fully mixing. The bubbles involved in the material mixing will make the liquid level rise, and the liquid level will fall again after the bubbles break. The vacuum degree, the viscosity of the glue and the requirements of the product are fixed (generally 2-4 minutes for defoaming). If there is no vacuum machine, the glue can be placed for 5-20 minutes in the clockwise direction for 2-3 minutes

4. Pour in the sealant and wait for curing: inject the necessary amount of sealant, and at the same time pay attention not to get involved in bubbles. After flowing into the bottom along the inner wall of the shell, let the glue level rise slowly and solidify at the set temperature








Why Choose us ?

1.Focus on the silicone material ,factory price and 100% quality gurantee,won many brand customers
2. Technical service support,professional after sales service on line
3.Oeko-tex,SGS certificate,no toxic,odorless
4.Quality raw material from brand supplier,all material test by standard lab
5.Professional research and product team,also our boss have more than 20 years experience in liquid silicone industry
6.Fast delivery,No worry after sales

Certificate
 


Company Profile

Focus on research & development, production, sales and technical services
Covers an area of more than 2,000 square meters
Won the trust of brand customers from domestic and overseas
Professional production team,also boss is a senior engineer whom have more than 20 years experience in the liquid silicone Industry.
Pass the Oeko-Tex & SGS

Exhibition


 

Send your message to this supplier

*From:
*To:
*Message:

Enter between 20 to 4,000 characters.

This is not what you are looking for? Post a Sourcing Request Now